Green Mortar for Submerged Arc Furnace

Characteristics
1. Easy to operate, no need to bake before use, reducing labor intensity for workers;
2. Better fluidity, easier to mud when blocking molten iron, can ensure the depth of blockage, and can protect the iron mouth brick well during long-term use;
3. Higher strength, more resistant to slag and iron erosion, smaller hole expansion during tapping process, stable tapping volume, and longer tapping time;
4. The choice of adhesive is more environmentally friendly and will not produce toxic gases during use
Specification /model
Model | Al2O3(%) | Water Content | Marshall Value(MPa) | CMOR(MPa) | CCS(MPa) | Bulk Density(g/cm3) |
220℃×24h | 220℃×24h | 220℃×24h | ||||
RH-L01 | ≥65 | ≤11 | <2.0 | ≥7.5 | ≥25 | ≥2.60 |
RH-L02 | ≥70 | ≤10 | <2.0 | ≥8.0 | ≥30 | ≥2.80 |
RH-L03 | ≥75 | ≤10 | <2.0 | ≥8.5 | ≥35 | ≥2.90 |
Packaging and Storage
25kg/box, store in a cool dry place to prevent hardening, use as soon as possible after opening, shelf life is six months.